I'll interpret my understanding of it the best I can. I am sure there are more scientific and technical descriptions out there.
Basically, a load of lumber that has already been kiln-dried to the usual 6-8% is loaded in a high-temperature kiln that can reach several hundred degrees. Your typical dry kiln can only reach temperatures of about 250 degrees F. It is stickered and stacked like a regular kiln charge. The oven/kiln reaches temperatures anywhere from 450-600 degrees F. Since wood will burn at this temperature, all the oxygen within the chamber must be removed with a vacuum.
The high temperature drives out the "bound" water in the wood's cells (the remaining 6-8% moisture content), effectively getting it as close to 0% moisture content as possible. The wood's cells have completely dried out at this point, and the openings in the cells where free water previously flowed in and out of the cells will be permanently closed. The cells can no longer take up moisture, which allow the manufacturers to advertise it as an excellent material for exterior trim, decks, etc. A light torreficiation process will produce a tan-colored tone. To get the darker tone of the Poplar shown above, the wood is left in there longer. In general, producers offer three shades - light, medium, and dark.
It's tough to find - my source for it no longer carries it. The most popular species are Poplar, Soft Maple, and Ash. Other woods have been attempted, but due to their structure, didn't respond as well as these three. If you ever come across some, I recommend giving it a try. It's more brittle than the regular specie, and a smooth finish can be a bit more difficult to achieve, but it's a nice conversation starter when someone asks if it's Walnut!